MARTENSITE / EN 1.4122
Description
Stainless steel MARTENSITE IN 1.4122 It is commonly known as X39CrMo17-1. This chromium-molybdenum alloy stands out for offering an excellent combination of high hardness and good wear resistance. Additionally, it provides improved corrosion protection compared to other martensitic grades with lower chromium content.
Furthermore, the EN 1.4122 It contains approximately 17% chromium along with molybdenum additions. For this reason, it is particularly suitable for slightly aggressive environments with low levels of chlorides. On the other hand, this steel is hardened through heat treatment of tempering and grinding. Consequently, it achieves considerable hardness while maintaining acceptable toughness. Similarly, it remains magnetic under all conditions.
Due to its great versatility in mechanical properties and chemical resistance, the use of this material is very common in engineering. As specialized distributors, we guarantee a certified supply with full technical traceability.
Applications in the real world
- High-quality cutlery (kitchen knives, professional cutting tools)
- Components of pumps and compressors (shafts, internal parts)
- Surgical and medical instruments that require hardness and resistance to sterilization
- Parts for machinery in the polymer processing industry
- Valves and accessories in moderately corrosive environments
- Components in the automotive and precision machinery industry
- Elements that require resistance to abrasion and a good surface finish
Quick View
| Property | Value (Typical) |
|---|---|
| Density | 7.70 g/cm³ |
| Hardness (Rebaked) | ≤ 280 HB |
| Hardness (Tempered) | 45–50 HRC |
| Magnetism | Yes (Ferromagnetic) |
| Equivalent | ASTM 440A / AISI 440C (Approximate) |
International Standards
- EN/DIN: 1.4122 (X39CrMo17-1)
- AFNOR: Z40CrMo17
- SIS: 2321
- UNI: X38CrMo17KW
Processing and Thermal Treatment
- Forging: 1100°C – 900°C (Slow cooling in sand or dry ash)
- Rebaked: 750°C – 820°C (Cooling in oven)
- Temple: 980°C – 1060°C (Cooling in oil or forced air)
- Returning: 650°C – 750°C (Air cooling to adjust mechanical properties)
- Relief of Tension: 600°C – 650°C (If necessary after heavy machining)

Useful links for EN 1.4122
- ASTM International Standards for Stainless Steels
- MatWeb Property Data for EN 1.4122
- AZoM Martensitic Stainless Steel Guide
You can also find the complete list of similar materials on the main page of Martensitic.