ASTM A182 F5: Chromium-molybdenum alloy steel for high temperature applications
The ASTM A182 F5 It is an alloy steel of chromium-molybdenum (5% Cr – 0.5% Mo) specifically designed for high-temperature and high-pressure service. This material offers excellent resistance to oxidation, high creep resistance, and remarkable durability in moderate corrosive environments. For these reasons, the ASTM A182 F5 es el estándar preferido para la fabricación de bridas, válvulas y accesorios forjados en refinerías y plantas petroquímicas donde la integridad estructural bajo calor extremo resulta crítica.
Technical properties of steel ASTM A182 F5
The physical and mechanical properties of this grade ensure great operational stability under severe working conditions. The following are detailed its main characteristics:
Property summary (Overview)
| Property | Value (Typical) |
|---|---|
| Density | 7.85 g/cm³ |
| Hardness (HBW) | 143 – 217 HB |
| Magnetism | Yes (Ferritic/Martensitic) |
| Thermal Conductivity | 24 W/(m·K) at 100°C |
Standards and equivalences
The standard ASTM A182 F5 It has various correspondences regarding key international regulations:
| DIN / EN | ASTM / Grade | UNS | Item number. |
|---|---|---|---|
| 12CrMo19-5 | A182 F5 | K41545 | 1.7362 |
Use and applications in the real world
Thanks to its chemical composition, the ASTM A182 F5 It is widely used in industrial sectors where materials resistant to heat are required. Its main applications include:
- Oil refineries: Components in catalytic cracking and distillation units that operate at high temperatures.
- Generation of Energy: Steam collectors, boiler pipes and components of high-pressure turbines.
- Chemical Industry: Heat exchangers and pressure vessels that handle hot fluids.
To learn how we process and prepare these materials, you can consult our metal cutting and processing services.
Processing and thermal treatment
Proper processing is indispensable to ensure the mechanical strength properties of the ASTM A182 F5:
- Forged: It requires a preheating between 900°C and 1200°C, followed by a forced cooling.
- Normalized and Revived: Heating to ≥955°C with cooling in air and subsequent annealing to ≥675°C to stabilize the microstructure.
- Total Reheat: Heating to ≥955°C followed by slow cooling within the oven.
- Welding: Although it is a weldable material, it requires preheating (200-300°C) and post-welding heat treatment (PWHT) to prevent cracking due to hardening.
International reference standards
The technical specifications of this alloy are covered by the following global regulations:
- EN/DIN: 1.7362 (12CrMo19-5)
- ASTM: A182 Grade F5
- ASME: SA182 Grade F5
- AFNOR: Z15CD5-05 (Approximate)
- JIS: SFVAF5
You can consult more official specifications about alloy regulations on the site of ASTM International Standards.
If you need to request a quote or require technical advice on ASTM A182 F5, Do not hesitate to get in touch Contact our sales team.